>> I heard about some people having problems with Poly Fiber just as I
was about to apply Top Gloss.  The UK distributor advised that the
problem was due to moisture content in the (UV) Smooth Prime.

This is a different problem to the disbond problem. If the moisture in
smooth prime is not allowed to vapourise out completely then any coating
you put on top can blister. The best thing to do is leave the Smooth
Prime for a month or so in warm weather to allow it to dry properly
before applying the top coating.